Nickel Chrome Heating Wire

Product Description

  Resistance wire(heating wire) used at operating temperatures up to 1200. Its chemical composition gives
 good oxidation resistance especially under conditions of frequent switching or wide temperature fluctuations.

 
  Applications include heating elements in both domestic and industrial appliances and in control resistors.
 Ni-Cr materials are widely used in industrial electric furnaces, household appliances and far-infrared devices
 because of their high temperature strength and strong plasticity.


Main property of NiCr  electric heating alloy
property  type Cr20Ni80 Cr30Ni70 Cr15Ni60 Cr20Ni35 Cr20Ni30
Main chemical
composition%
Ni Rest Rest 55~61 34~37 30~34
Cr 20~23 28~31 15~18 18~21 18~21
Fe

Rest Rest Rest
Max continuous
 Temp.of element(
)
1200 1200 1150 1100 1100
resistivity(mm²/m) 1.09 1.09 1.12 1 1.04
Density((g/cm³)) 8.4 8.4 8.2 7.9 7.9
Thermal conductivity(KJ/M.h) 60.3 60.3 45.2 43.8 43.8
Coefficient of liner
expansion(a*10-5/
)
18 18 17 19 19
Melting point () 1400 1400 1390 1390 1390
Elongation(%) 720 720 720 720 720
Micrographic structure Austenitic Austenitic Austenitic Austenitic Austenitic
Magnetic property NONE NONE NONE NONE NONE


Technical Data Sheet

 
    Main characteristics of Ni-Cr electric heating alloys
   
                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                                       
         Alloy Nomenclature/Performance          Cr20Ni80          Cr30Ni70          Cr15Ni60          Cr20Ni35          Cr20Ni30
         Main
         Chemical
          composition
         Ni          Rest          Rest          55.0-61.0          34.0-37.0          30.0-34.0
         Cr          20.0-23.0          28.0-31.0          15.0-18.0          18.0-21.0          18.0-21.0
         Fe          ≤1.0          ≤1.0          Rest          Rest          Rest
         Max. continuous service temp. of element                    1200          1250          1150          1100          1100
         Resistivity at 20°C(μΩ·m)                    1.09          1.18          1.12          1          1.04
         Density (g/cm3)                    8.4          8.1          8.2          7.9          7.9
         Thermal conductivity(KJ/m·h·°C)                    60.3          45.2          45.2          43.8          43.8
         Coefficient of lines expansion(α×10-6/°C)                    18          17          17          19          19
         Melting point (approx.)( °C)                    1400          1380          1390          1390          1390
         Elongation at rupture (%)                    >20          >20          >20          >20          >20
         Micrographic structure                    austenite          austenite          austenite          austenite          austenite
         Magnetic properties                    nonmagnetic          nonmagnetic          nonmagnetic          Weak magnetic          Weak magnetic